The role of annealing temperature on the optical energy gap and Urbach energy of Se:2%Sb thin films
Main Article Content
Abstract
The optical energy gap(Eopt) and the width of the tails of localized states in the band gap (?E) for Se:2%Sb thin films prepared by thermal co-evaporation method as a function of annealing temperature are studied in the photon energy range ( 1 to 5.4)eV.Se2%Sb film was found to be indirect transition with energy gap of (1.973,2.077, 2.096, 2.17) eV at annealing temperature (295,370,445,520)K respectively.
The Eopt and ?E of Se:2%Sb films as a function of annealing temperature showed an increase in Eopt and a decrease in ?E with increasing the annealing temperature. This behavior may be related to structural defects and dangling bonds.
The Eopt and ?E of Se:2%Sb films as a function of annealing temperature showed an increase in Eopt and a decrease in ?E with increasing the annealing temperature. This behavior may be related to structural defects and dangling bonds.
Article Details
How to Cite
1.
The role of annealing temperature on the optical energy gap and Urbach energy of Se:2%Sb thin films . Baghdad Sci.J [Internet]. 2008 Jun. 1 [cited 2024 Dec. 19];5(2):249-52. Available from: https://bsj.uobaghdad.edu.iq/index.php/BSJ/article/view/894
Section
article
How to Cite
1.
The role of annealing temperature on the optical energy gap and Urbach energy of Se:2%Sb thin films . Baghdad Sci.J [Internet]. 2008 Jun. 1 [cited 2024 Dec. 19];5(2):249-52. Available from: https://bsj.uobaghdad.edu.iq/index.php/BSJ/article/view/894