Studying The Optical Properties of CdO and CdO: Bi Thin Films

Main Article Content

Zain A. Muhammad
Ahmed T. Hassan
Yasmeen Z. Dawood

Abstract

Cadmium Oxide and Bi doped Cadmium Oxide thin films are prepared by using the chemical spray pyrolysis technique a glass substrate at a temperature of (400?C) with volumetric concentration (2,4)%. The thickness of all prepared films is about (400±20) nm. Transmittance and Absorbance spectra are recorded in the wave length ranged (400-800) nm. The nature of electronic transitions is determined, it is found out that these films have directly allowed transition with an optical energy gap of (2.37( eV for CdO and ) 2.59, 2.62) eV for (2% ,4%) Bi doped CdO respectively. The optical constants have been evaluated before and after doping.

Article Details

How to Cite
1.
Studying The Optical Properties of CdO and CdO: Bi Thin Films. Baghdad Sci.J [Internet]. 2016 Sep. 4 [cited 2024 Nov. 25];13(3):0593. Available from: https://bsj.uobaghdad.edu.iq/index.php/BSJ/article/view/2303
Section
article

How to Cite

1.
Studying The Optical Properties of CdO and CdO: Bi Thin Films. Baghdad Sci.J [Internet]. 2016 Sep. 4 [cited 2024 Nov. 25];13(3):0593. Available from: https://bsj.uobaghdad.edu.iq/index.php/BSJ/article/view/2303

Similar Articles

You may also start an advanced similarity search for this article.